英语翻译:

1.定位焊缝存在弧坑裂纹,在正式焊接之前请打磨这些定位焊缝,以确保焊缝质量。定位焊缝请勿使用手工电弧焊(贵公司未提供手工电弧焊焊接工艺)。1.在组对之前请将坡口及其两侧的... 1. 定位焊缝存在弧坑裂纹,在正式焊接之前请打磨这些定位焊缝,以确保焊缝质量。定位焊缝请勿使用手工电弧焊(贵公司未提供手工电弧焊焊接工艺)。
1. 在组对之前请将坡口及其两侧的铁锈、油污等影响焊接质量的因素清理干净,露出金属光泽。
1. 纵筋与隔板组对位置与图纸不符。
隔板没开过焊孔。
盖板与腹板垂直度过大,不符合要求(H/200,≦3mm)
展开
xxxxxxxxxxxxxxxxxxx2
2014-03-31 · 超过11用户采纳过TA的回答
知道答主
回答量:73
采纳率:0%
帮助的人:25.2万
展开全部
1.定位焊缝存在弧坑裂纹,在正式焊接之前请打磨这些定位焊缝,以确保焊缝质量。定位焊缝请勿使用手工电弧焊(贵公司未提供手工电弧焊焊接工艺)。
Crater crack exists 1 positioning weld, welding in formal before grinding these positioning weld, to ensure the quality of welding seam. Tack welds do not use manual arc welding (your company did not provide manual arc welding process).
1. 在组对之前请将坡口及其两侧的铁锈、油污等影响焊接质量的因素清理干净,露出金属光泽。1. 纵筋与隔板组对位置与图纸不符。隔板没开过焊孔。盖板与腹板垂直度过大,不符合要求(H/200,≦3mm)
1 in the group of factors on both sides before groove and rust, oil, welding quality is clean, with metallic luster. 1 longitudinal reinforcement and the partition does not match the position and drawing of group. Partition have not opened a hole. The cover plate and the web plate vertically through the large, do not meet the requirements of (H/200, 3mm)
已赞过 已踩过<
你对这个回答的评价是?
评论 收起
Catherine_Kwok
2014-03-31 · TA获得超过368个赞
知道答主
回答量:135
采纳率:0%
帮助的人:94.8万
展开全部
Longitudinal reinforcement and
the baffle group does not comply with drawings on location. Spend the large
cover plate perpendicular to the Web, does not meet the requirements (H/200, ≦ 3mm)

There are some visible arc crack
on position-oriented welding. To ensure the welding quality, polish processing are requested
to be added before the final welding. position-oriented welding do not use
manual arc welding (your company did not provide a manual arc welding process).

Please clean up the rust , greasy dirt of two side of groove and
other influence factors that may caused welding quality issues before group
welding.

Longitudinal reinforcement and
the baffle group does not comply with drawings. Bulkhead didn't open welding
holes.

Squareness of cover plate and Web
it’s doesn’t meet the requirements. (H/200, ≦ 3mm)
已赞过 已踩过<
你对这个回答的评价是?
评论 收起
航哥享学
2014-03-31 · TA获得超过200个赞
知道小有建树答主
回答量:281
采纳率:33%
帮助的人:104万
展开全部
1,Weld locating gap has crack and dent mark, make sure to polish them smooth before welding taken place, so that to achieve good weld line quality. do not use manual electric arc welder to locate weld slot (your company has not provide manual arc welding technique instructions).
2, Clean oil, iron rust, and other dirty factors near or aside of ramp cut openning, to avoid affect welding quality. be sure to expose metalic shinng before matching.
3, The matching location between cross ribs and baffle plates are different from drawing.
Baffle plate has no welding hole prepared.

The verticality of cover plate and laying plate is too big, inacceptable (H/200,≦3mm
)
原创。抄袭者受咒
已赞过 已踩过<
你对这个回答的评价是?
评论 收起
yy6891
2014-03-31 · TA获得超过5331个赞
知道大有可为答主
回答量:2586
采纳率:0%
帮助的人:1526万
展开全部
  1. Crater crack are found in tack weldings.Please polish those tack weldings before official welding to secure the quality.Please donot apply manual arc welding when tack welding(your company didn't provide manual telding technique)

  2. Please clear the groove and rust and greasy dirt that might affect the welding quality before fitting up.

  3. Fitting up location of  longitudinal bar and clapboard dosent match with the drawings


There are no welding holes on the clapboards

The rectangularity between the cover board and the web board is too large,which is not confirm to the requirements

本回答被提问者采纳
已赞过 已踩过<
你对这个回答的评价是?
评论 收起
收起 更多回答(2)
推荐律师服务: 若未解决您的问题,请您详细描述您的问题,通过百度律临进行免费专业咨询

为你推荐:

下载百度知道APP,抢鲜体验
使用百度知道APP,立即抢鲜体验。你的手机镜头里或许有别人想知道的答案。
扫描二维码下载
×

类别

我们会通过消息、邮箱等方式尽快将举报结果通知您。

说明

0/200

提交
取消

辅 助

模 式